中空玻璃二道密封的常用設備--雙組份打膠機
時(shí)間:2019-03-29 來(lái)源:http://ruiyingjituan.com/ 發(fā)布人:昌盛機械
雙組份打膠機是完成中空玻璃二道密封的專(zhuān)用設備,在運用過(guò)程中可能會(huì )呈現形形色色的問(wèn)題,濟南昌盛機械的售后服務(wù)人員,分離多年調試和客戶(hù)實(shí)踐消費的經(jīng)歷,對雙組份打膠機在運用和維護方面總結了以下幾點(diǎn)經(jīng)驗,整理成以下小文,希望可以協(xié)助進(jìn)入中空玻璃加工行業(yè)的朋友。
Two-component glue beater is a special equipment to complete two-way sealing of hollow glass, which may present various problems in the operation process. After-sales service personnel of Jinan Xingsheng Machinery have separated many years'experience of debugging and customer's practical consumption. This paper summarizes the following experiences in the application and maintenance of two-component glue beater, and arranges them into the following articles in the hope of assisting in entering hollow glass. Friends of glass processing industry.
雙組份打膠機常見(jiàn)毛病現象和處理辦法:
Common faults of two-component glue beater and treatment methods:
1、打膠機壓盤(pán)冒膠
1. Rubber tapping from press plate of glue beater
①升降壓力太大。
The lifting pressure is too high.
②桶太大了,不適宜,客戶(hù)在采購時(shí),先量一下本人的打膠機壓盤(pán)大小,如今市面上機器壓盤(pán)有三個(gè)規格的,560mm,565mm,571mm.
(2) The barrel is too big to be suitable. When purchasing, the customer first measures the size of the press plate of his gluing machine. Now there are three specifications of the press plate on the market, 560mm, 565mm and 571mm.
③壓盤(pán)密封圈損壞變形,老化發(fā)硬,改換新的膠圈。
(3) Damage and deformation of pressure disk sealing ring, aging and hardening, replacement of new rubber ring.
2、混合不勻,呈現白絲,花膠
2. Uneven mixing, white silk, gum
①空壓機空氣壓力缺乏,氣量不穩,調整壓力。
The air compressor is short of air pressure, the air volume is unstable, and the pressure is adjusted.
②打膠機比例泵內有臟物,清洗比例泵。
(2) There are viscera in the proportioning pump of the glue beater, and the proportioning pump is cleaned.
③打膠機混合器單向閥走漏,改換單向閥。
(3) The one-way valve of mixer of glue beater leaks out and replaces the one-way valve.
④打膠機混合器及槍內通道局部梗塞,清洗混合器和管道。
(4) Local infarction in mixer and gun passage of glue beater, cleaning mixer and pipeline.
3、固化速度太快或太慢
3. Curing speed is too fast or too slow
①夏季氣溫較高,膠固化的速度會(huì )快一點(diǎn),可依據狀況,把比例尺往數字大的方向調一點(diǎn)→(10,11,12,13,14),冬季氣溫較低,膠的固化速度會(huì )慢一點(diǎn),可依據狀況,把比例尺調小一點(diǎn)→(9,8,7,6)
(1) Higher temperature in summer, faster curing speed of glue. According to the situation, we can adjust the scale to the direction of big numbers (10, 11, 12, 13, 14), lower temperature in winter, slower curing speed of glue. According to the situation, we can reduce the scale to (9, 8, 7, 6).
②A(yíng)、B組份比例未調理好,A、B組份比例應按10:1(體積比)停止混合。各個(gè)打膠機比例表尺上顯現的比例和實(shí)踐出膠的比例有偏向,有的打膠機調到14:1,可是實(shí)踐出來(lái)的只要10:1,所以這一點(diǎn)就要靠操作人員去判別,一桶A組份膠(白膠)是剛好配一桶B組份膠(黑膠)。假如B膠用得多,膠干得快,把比例尺向大的數字調→(10、11、12、13、14),假如B膠用得少(膠干得慢,不夠黑,發(fā)灰),把比例向小的數字調→(9、8、7、6)。
(2) The proportion of component A and B is not adjusted properly, and the proportion of component A and B should stop mixing at 10:1 (volume ratio). There is a bias between the proportion shown on the scale of each glue beater and the proportion of glue produced in practice. Some glue beaters are adjusted to 14:1, but only 10:1 is needed in practice. Therefore, it depends on operators to distinguish this point. A barrel of component A glue (white glue) is just matched with a barrel of component B glue (black glue). If B glue is used more, it dries faster, adjust the scale to the larger number (10, 11, 12, 13, 14), if B glue is used less (slow drying, not dark enough, gray), adjust the proportion to the smaller number (9, 8, 7, 6).
今天由濟南昌盛雙組份打膠機大家分享的內容就到這里了,想要了解更多關(guān)于雙組份打膠機的具體情況,歡迎咨詢(xún)我們官網(wǎng)的在線(xiàn)客服人員:http://linshi.jncsjx.com我們將會(huì )盡快給您做出回復,謝謝大家的支持。
Today, the content shared by everyone of Jinan Changsheng two-component glue punch is here. For more information about the two-component glue punch, please consult our online customer service staff on the official website: http://linshi.jncsjx.com. We will reply to you as soon as possible. Thank you for your support.
- STJ03B型雙組份打膠機的性能和結構特點(diǎn) 2024/07/13
- 全自動(dòng)鋁條折彎機鋁框自動(dòng)打標技術(shù) 2024/07/11
- 中空玻璃打膠的好壞與哪些方面有關(guān)系? 2024/07/09
- 中空玻璃生產(chǎn)線(xiàn)和復合膠條中空玻璃生產(chǎn)線(xiàn)區別? 2024/07/04
- 中空玻璃加工設備故障分析流程 2024/07/03
- 中空玻璃加工設備的現場(chǎng)安裝事項要點(diǎn) 2024/06/27
- 中空玻璃的生產(chǎn)過(guò)程是怎樣的? 2024/06/24
- 中空玻璃生產(chǎn)線(xiàn)的構造及功能介紹 2024/06/19
- 中空玻璃生產(chǎn)線(xiàn)有哪些設備組成 2024/06/13
- 丁基涂布機的膠嘴漏膠會(huì )不會(huì )營(yíng)銷(xiāo)生產(chǎn)質(zhì)量? 2024/06/13
產(chǎn)品分類(lèi)Product categories
聯(lián)系我們Contact us
- 咨詢(xún)熱線(xiàn):0531-85717458 13705446998
- 公司地址: 山東省德州市齊河安頭鄉企巢工業(yè)園